Q and e Experimental valuesa
Vinyl
Monomer |
Q |
e |
Acrylic Acid |
0.76 |
1.11 |
Acrylonitrile |
0.40 |
0.91 |
α-Methylstyrene |
0.98 |
-1.04 |
Butadiene |
1.66 |
-0.59 |
Diethyl Fumarate |
0.24 |
2.26 |
Ethyl vinyl ether |
0.03 |
-1.49 |
Hydroxyethyl methacrylate |
0.87 |
0.30 |
Hydroxypropyl acrylate |
0.92 |
0.75 |
Maleic anhydride |
0.55 |
2.97 |
Methacrylic acid |
1.66 |
0.64 |
Methacrylonitrile |
0.86 |
0.69 |
Methyl acrylate |
0.31 |
0.50 |
Methyl methacylate |
0.57 |
0.30 |
n-Butyl acrylate |
0.32 |
0.74 |
Styrene |
1.00 |
-0.80 |
t-Butyl methacrylate |
0.74 |
0.24 |
t-Butyl vinyl ether |
0.15 |
-1.58 |
Vinyl acetate |
0.02 |
-0.28 |
Vinyl chloride |
0.13 |
0.07 |
Vinyl methyl ketone |
0.68 |
0.87 |
Vinylidene chloride |
0.20 |
0.24 |