Activation Energy For the Initiator Dissociation
Initiator |
Ea (kJ/mol) |
2,3-Dimethyl-2,3-diphenylbutane |
212.6 |
1,1,3,3-Tetramethylbutyl
hydroperoxide |
182.0 |
tert-Butyl hydroperoxide |
167.5 |
Di(tert-butyl)peroxide |
152.7 |
2,5-Dimethyl-2,5-di(tert-butylperoxy)hexyne-3 |
152.3 |
Dicumyl peroxide |
152.3 |
tert-Amyl peroxyacetate |
152.2 |
tert-Butyl cumyl
peroxide |
150.5 |
3,6,9-Triethyl-3,6,9-trimethyl-1,4,7-triperoxonane |
150.2 |
tert-Butylperoxy
isopropyl carbonate |
150.2 |
tert-Amylperoxy-(2-ethylhexyl)carbonate |
149.7 |
tert-Butylperoxy-acetate |
149.2 |
2,5-Dimethyl-2,5-di(tert-butylperoxy)hexane |
148.7 |
2,2-Di(tert-butylperoxy)butane |
148.5 |
Di(tert-butylperoxy-isopropyl)benzene |
147.3 |
tert-Butylperoxybenzoate |
147.3 |
tert-Amyl
peroxy-benzoate |
145.0 |
tert-Butyl
peroxy-3,5,5-trimethyl-hexanoate |
143.9 |
Butyl
4,4-di(tert-butylperoxy)valerate |
143.5 |
Di(3-methoxybutyl)
peroxydicarbonate |
143.3 |
1,1’-Azodi(hexahydrobenzonitrile) |
142.2 |
1,1-Di(tert-butylperoxy)cyclohexane |
140.2 |
tert-Butylperoxy-(2-ethylhexyl)carbonate |
139.9 |
1,1-Di(tert-amylperoxy)cyclohexane |
139.5 |
Di-(tert-amyl)-peroxide |
138.7 |
1,1-Di(tert-butylperoxy)-3,5,5-trimethylcyclohexane |
135.3 |
Ammoniumperoxodisulfate |
135.0 |
tert-Butyl
peroxydiethylacetate |
134.0 |
2,5-Dimethyl-2,5-di(2-ethylhexanoylperoxy)hexane |
133.9 |
tert-Butyl
peroxy-isobutyrate |
132.6 |
Cumyl hydroperoxide |
132.6 |
Isopropylcumyl
hydroperoxide |
131.4 |
Isopropylcumyl
hydroperoxide |
131.4 |
2,2’-Azodi(isobutyronitrile) |
130.1 |
tert-Butyl
peroxy-2-ethylhexanoate |
130.0 |
tert-Amyl
peroxy-2-ethylhexanoate |
129.1 |
2,2’-Azodi(2-methylbutyronitrile) |
128.9 |
Didecanoyl peroxide |
128.2 |
Di(4-tert-butylcyclohexyl)
peroxydicarbonate |
126.4 |
Di(4-methylbenzoyl)peroxide |
125.0 |
tert-Amyl peroxypivalate |
124.4 |
Dicetyl
peroxydicarbonate |
124.3 |
Dibenzoyl peroxide |
124.2 |
Dimyristyl
peroxydicarbonate |
124.1 |
Diisopropyl
peroxydicarbonate |
124.0 |
Di-sec-butyl
peroxydicarbonate |
123.9 |
1,1,3,3-Tetramethylbutyl
peroxy-2-ethylhexanoate |
123.8 |
Dilauroyl peroxide |
123.4 |
Di(3,5,5-trimethylhexanoyl)
peroxide |
122.7 |
Di(2-ethylhexyl)
peroxydicarbonate |
122.5 |
tert-Butyl
peroxyneodecanoate |
118.2 |
1,1,3,3-Tetramethylbutyl
peroxypivalate |
117.5 |
tert-Butyl
peroxypivalate |
116.8 |
tert-Butyl
peroxyneoheptanoate |
116.8 |
1,1,3,3-Tetramethylbutyl
peroxyneodecanoate |
116.4 |
tert-Butyl-monoperoxy-maleate |
116.0 |
Cumyl peroxyneodecanoate |
114.8 |
Cumyl
peroxyneoheptanoate |
114.3 |
tert-Amyl
peroxyneodecanoate |
113.7 |
Diisobutyryl peroxide |
109.1 |