Monomer |
Structure |
MW (g/mol) |
Tg (°C) |
Methyl Methacrylate (MMA) |
|
100.1 |
105 |
Methacrylic acid (MAA) |
|
86.1 |
185 |
n-Butyl methacrylate (n-BMA) |
|
142.2 |
20 |
i-Butyl methacrylate (i-BMA) |
|
142.2 |
53 |
Lauryl methacrylate (LMA) |
|
254 |
-62.5 |
Stearyl Methacrylate (SMA) |
|
338 |
38.5 |
Benzyl methacrylat (BNMA)e |
|
176 |
54 |
Cyclohexyl methacrylate (CHMA) |
|
168.2 |
107 |
Isobornyl methacrylate (IBOMA) |
|
222.3 |
110.5 |
2-Ethylhexyl methacrylate (2-EHMA) |
|
198.3 |
-10 |
Tetrahydrofurfuryl Methacrylate (THFMA) |
|
170.2 |
43.5 |
2-Hydroxyethyl methacrylate (HEMA) |
|
130.1 |
55 |
Hydroxypropyl methacrylate (HPMA) |
|
144.2 |
73 |