Poly(vinyl valerate)
CROW logo
Poly(vinyl valerate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyvinylester
COMMON NAMESPoly(vinyl valerate)
STRUCTURE BASED NAME Poly(valeroyloxyethylene), Poly(pentanoyloxyethylene)
ACRONYMS  
CAS #  
CurlySMILES C{-}C{n+}(OC(=O)CCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 227-533-3
COMMON NAMESVinyl valerate, Ethenyl pentanoate
SMILES CCCCC(=O)OC=C
Std. InChI 1S/C7H12O2/c1-3-5-6-7(8)9-4-2/h4H,2-3,5-6H2,1H3
Std. InChIKey BLZSRIYYOIZLJL-UHFFFAOYSA-N
STRUCTURE
Vinyl valerate
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1 118.51 
Density ρg mL-1 1.081 
Solubility Parameter δMPa1/2   
Molar Cohesive Energy EcohJ mol-1   
Glass Transition Temperature TgK   
Molar Heat Capacity CpJ (mol K)-1   
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone   
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 128.17
Van-der-Waals Volume VvWmL mol-1 76.8
Molar Volume VmmL mol-1 117 - 121118
Density ρ g mL-1 1.06 - 1.10 1.08
Solubility Parameter δMPa1/2 18.1 - 19.018.4
Molar Cohesive Energy EcohJ mol-1 38000 - 4200040000
Glass Transition Temperature TgK 245 -253248
Molar Heat Capacity CpJ (mol K)-1 242 - 248246
Entanglement Molecular Weight Meg mol-1 16500 - 1850018000
Index of Refraction nnone 1.47 - 1.491.48

 1Interpolated values;   Last updated: December 4, 2016