Poly(propyl vinyl thioether)
CROW logo
Poly(propyl vinyl thioether)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyvinylsulfide
COMMON NAMESPoly(propyl vinyl thioether), Poly(vinyl propyl sulfide)
STRUCTURE BASED NAME Poly(propylthioethylene)
ACRONYMS
CAS #
CurlySMILES C{-}C{n+}(SCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 16330-21-5
COMMON NAMESPropyl vinyl thioether, 1-(Vinylsulfanyl)propane
SMILES CCCSC=C
Std. InChI 1S/C5H10S/c1-3-5-6-4-2/h4H,2-3,5H2,1H3
Std. InChIKey HWRMMWBUMQCMJK-UHFFFAOYSA-N
STRUCTURE
Propyl vinyl thioether
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1 99.91 
Density ρg mL-1 1.021 
Solubility Parameter δMPa1/2   
Molar Cohesive Energy EcohJ mol-1   
Glass Transition Temperature TgK  
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Me g mol-1
Index of Refraction nnone
1Interpolated
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 102.2
Van-der-Waals Volume VvWmL mol-1 61.3
Molar Volume VmmL mol-1 99.5 - 100.399.9
Density ρg mL-1 1.02 - 1.031.02
Solubility Parameter δMPa1/2 17.3 - 17.917.6
Molar Cohesive Energy EcohJ mol-1 29800 - 3210031000
Glass Transition Temperature TgK 236 - 265253
Molar Heat Capacity CpJ (mol K)-1 192 - 200195
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone 1.54 - 1.551.54