POLYMER CLASS | Polyvinylester |
COMMON NAMES | Poly(vinyl propionate), Vinyl propionate polymer |
STRUCTURE BASED NAME | Poly(propionyloxyethylene) |
ACRONYMS | |
CAS # | |
CurlySMILES | C{-}C{n+}(OC(=O)CC) |
CAS # | 105-38-4 |
COMMON NAMES | Vinyl propionate |
SMILES | C=COC(=O)CC |
Std. InChI | 1S/C5H8O2/c1-3-5(6)7-4-2/h4H,2-3H2,1H3 |
Std. InChIKey | UIWXSTHGICQLQT-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 89.0 - 90.2 | 89.6 |
Density ρ | g mL-1 | 1.11 - 1.12 | 1.12 |
Solubility Parameter δ | MPa1/2 | 18.0 - 20.0 | 18.6 |
Molar Cohesive Energy Ecoh | J mol-1 | 28200 - 34400 | 31100 |
Glass Transition Temperature Tg | K | 283 | |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.47 |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 100.12 | |
Van-der-Waals Volume VvW | mL mol-1 | 56.2 | |
Molar Volume Vm | mL mol-1 | 84.4 - 87.9 | 86.1 |
Density ρ | g mL-1 | 1.14 - 1.19 | 1.16 |
Solubility Parameter δ | MPa1/2 | 18.7 - 19.6 | 19.1 |
Molar Cohesive Energy Ecoh | J mol-1 | 29400 - 33100 | 31300 |
Glass Transition Temperature Tg | K | 273 - 309 | 288 |
Molar Heat Capacity Cp | J (mol K)-1 | 140 - 150 183 - 190 | 144 (s) 185 (l,r) |
Entanglement Molecular Weight Me | g mol-1 | 9600 - 11300 | 10500 |
Index of Refraction n | none | 1.46 - 1.49 | 1.48 |