Poly(vinyl phenyl sulfide)
CROW logo
Poly(vinyl phenyl sulfide)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyvinylsulfide
COMMON NAMESPoly(vinyl phenyl sulfide), Poly(phenylthioethene)
STRUCTURE BASED NAME Poly[(vinylsulfanyl)benzene]
ACRONYMS
CAS #
CurlySMILES C{-}C{n+}(Sc1ccccc1)
 

IDENTIFIERS OF MONOMER(S)

CAS # 1822-73-7
COMMON NAMESVinyl phenyl sulfide, Phenylthioethene, (Vinylsulfanyl)benzene [
SMILES C=CSc1ccccc1
Std. InChI 1S/C8H8S/c1-2-9-8-6-4-3-5-7-8/h2-7H,1H2
Std. InChIKey GMPDOIGGGXSAPL-UHFFFAOYSA-N
STRUCTURE
Vinyl phenyl sulfide
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1118.0 - 118.4118.2
Density ρg mL-1 1.151.15
Solubility Parameter δMPa1/2 18.2 - 20.419.3
Molar Cohesive Energy EcohJ mol-1 38400 - 48200 44000
Glass Transition Temperature TgK 386
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone1.55 - 1.661.66
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 136.22
Van-der-Waals Volume VvWmL mol-1 76.21
Molar Volume VmmL mol-1113.7 - 117.7117.0
Density ρg mL-1 1.16 - 1.20 1.16
Solubility Parameter δMPa1/2 19.3 - 20.419.9
Molar Cohesive Energy EcohJ mol-1 43900 - 4710046400
Glass Transition Temperature TgK 398
Molar Heat Capacity CpJ (mol K)-1149 - 158152
Entanglement Molecular Weight Meg mol-122800
Index of Refraction nnone1.65 - 1.661.65
back to top