POLYMER CLASS | Polyvinylsulfide |
COMMON NAMES | Poly(methyl vinyl thioether), Poly(vinyl methyl sulfide) |
STRUCTURE BASED NAME | Poly(methylthioethylene) |
ACRONYMS | |
CAS # | |
CurlySMILES | C{-}C{n+}(SC) |
CAS # | 1822-74-8 |
COMMON NAMES | Methyl vinyl thioether, (Methylthio)ethene |
SMILES | CSC=C |
Std. InChI | 1S/C3H6S/c1-3-4-2/h3H,1H2,2H3 |
Std. InChIKey | AMBKPYJJYUKNFI-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 66.6 - 67.0 | 66.8 |
Density ρ | g mL-1 | 1.11 | 1.11 |
Solubility Parameter δ | MPa1/2 | 17.5 - 20.7 | 19.1 |
Molar Cohesive Energy Ecoh | J mol-1 | 20300 - 28400 | 24400 |
Glass Transition Temperature Tg | K | 272 | |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 74.15 | |
Van-der-Waals Volume VvW | mL mol-1 | 40.77 | |
Molar Volume Vm | mL mol-1 | 64.7 - 67.6 | 66.3 |
Density ρ | g mL-1 | 1.10 - 1.15 | 1.12 |
Solubility Parameter δ | MPa1/2 | 17.8 - 18.6 | 18.1 |
Molar Cohesive Energy Ecoh | J mol-1 | 21000 - 23300 | 21700 |
Glass Transition Temperature Tg | K | 266 - 273 | 270 |
Molar Heat Capacity Cp | J (mol K)-1 | 130 - 141 | 134 |
Entanglement Molecular Weight Me | g mol-1 | 5800 - 8500 | 7200 |
Index of Refraction n | none | 1.57 - 1.59 | 1.58 |