Poly(vinyl isobutyl ether)
CROW logo
Poly(vinyl isobutyl ether)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyvinylether
COMMON NAMESPoly(vinyl isobutyl ether), Poly(isobutyl vinyl ether)
STRUCTURE BASED NAME Poly(isobutoxyethylene)
ACRONYMS
CAS #
CurlySMILES C{-}C{n+}(OCC(C)C)
 

IDENTIFIERS OF MONOMER(S)

CAS # 109-53-5
COMMON NAMESIsobutyl vinyl ether
SMILES C=COCC(C)C
Std. InChI 1S/C6H12O/c1-4-7-5-6(2)3/h4,6H,1,5H2,2-3H3
Std. InChIKey OZCMOJQQLBXBKI-UHFFFAOYSA-N
STRUCTURE
Isobutyl vinyl ether
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1107.6 - 111.3109.4
Density ρg mL-1 0.90 - 0.930.92
Solubility Parameter δMPa1/2 16.6 - 19.217.9
Molar Cohesive Energy EcohJ mol-1 29300 - 39100 35100
Glass Transition Temperature TgK 254 - 255255
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone1.45
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 100.16
Van-der-Waals Volume VvWmL mol-1 63.65
Molar Volume VmmL mol-1109.2 - 109.5109.4
Density ρg mL-1 0.91 - 0.920.92
Solubility Parameter δMPa1/2 16.2 - 17.416.7
Molar Cohesive Energy EcohJ mol-1 28900 - 3100030400
Glass Transition Temperature TgK 241 - 255248
Molar Heat Capacity CpJ (mol K)-1204 - 216209
Entanglement Molecular Weight Meg mol-111000 - 1360012300
Index of Refraction nnone1.45 - 1.471.45
back to top