POLYMER CLASS | Polyhaloolefins |
COMMON NAMES | Poly(vinylidene chloride), Saran™ |
STRUCTURE BASED NAME | Poly(1,1-dichloroethylene) |
ACRONYMS | PVDC |
CAS # | 9002-85-1 |
CurlySMILES | C{-}(Cl)(Cl)C{n+} |
CAS # | 75-35-4 |
COMMON NAMES | 1,1-Dichloroethene |
SMILES | ClC(=C)Cl |
Std. InChI | 1S/C2H2Cl2/c1-2(3)4/h1H2 |
Std. InChIKey | LGXVIGDEPROXKC-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 54.6 - 58.8 | 56.6 |
Density ρ | g mL-1 | 1.65 - 1.78 | 1.71 |
Solubility Parameter δ | MPa1/2 | 18.9 - 21.3 | 20.6 |
Molar Cohesive Energy Ecoh | J mol-1 | 20700 - 26200 | 24600 |
Glass Transition Temperature Tg | K | 255 - 258 280 - 288 | 256 284 |
Molar Heat Capacity Cp | J (mol K)-1 | 130 | |
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.60 - 1.63 | 1.62 |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 96.94 | |
Van-der-Waals Volume VvW | mL mol-1 | 37.07 | |
Molar Volume Vm | mL mol-1 | 54.9 - 58.1 | 56.8 |
Density ρ | g mL-1 | 1.67 - 1.77 | 1.71 |
Solubility Parameter δ | MPa1/2 | 19.9 - 20.2 | 20.0 |
Molar Cohesive Energy Ecoh | J mol-1 | 23200 - 22500 | 22800 |
Glass Transition Temperature Tg | K | 254, 295 | |
Molar Heat Capacity Cp | J (mol K)-1 | 104 - 117 | 112 |
Entanglement Molecular Weight Me | g mol-1 | 18000 - 25800 | 14600 |
Index of Refraction n | none | 1.58 - 1.62 | 1.61 |
Last updated: March 18, 2017