Poly(vinyl caproate)
CROW logo
Poly(vinyl caproate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyvinylester
COMMON NAMESPoly(vinyl caproate)
STRUCTURE BASED NAME Poly(vinyl hexanoate), Poly[1-(hexanoyloxy)ethylene]
ACRONYMS  
CAS #  
CurlySMILES C{-}C{n+}(OC(=O)CCCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 221-265-0
COMMON NAMESVinyl caproate, Vinyl hexanoate
SMILES CCCCCC(=O)OC=C
Std. InChI 1S/C8H14O2/c1-3-5-6-7-8(9)10-4-2/h4H,2-3,5-7H2,1H3
Std. InChIKey LZWYWAIOTBEZFN-UHFFFAOYSA-N
STRUCTURE
Vinyl caproate
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1 1331 
Density ρg mL-1 1.071 
Solubility Parameter δMPa1/2   
Molar Cohesive Energy EcohJ mol-1   
Glass Transition Temperature TgK   
Molar Heat Capacity CpJ (mol K)-1   
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone   
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unit g mol-1 142.2
Van-der-Waals Volume VvWmL mol-1 87.0
Molar Volume VmmL mol-1 133 - 137134.5
Density ρg mL-1 1.03- 1.071.06
Solubility Parameter δMPa1/2 17.9 - 18.818.2
Molar Cohesive Energy EcohJ mol-1 43000 - 4700045000
Glass Transition Temperature TgK 232 - 240236
Molar Heat Capacity CpJ (mol K)-1 271 - 280276
Entanglement Molecular Weight Meg mol-1 21000 - 2300022000
Index of Refraction n none 1.47 - 1.491.48

 1Interpolated values;   Last updated: December 4, 2016