NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyhaloolefins
COMMON NAMESPoly(vinyl bromide)
STRUCTURE BASED NAME Poly(bromoethylene)
ACRONYMS
CAS # 25951-54-6
CurlySMILES C{-}(Br)C{n+}
 

IDENTIFIERS OF MONOMER(S)

CAS # 25951-54-6
COMMON NAMESBromoethene
SMILES BrC=C
Std. InChI 1S/C2H3Br/c1-2-3/h2H,1H2
Std. InChIKey INLLPKCGLOXCIV-UHFFFAOYSA-N
STRUCTURE
Bromoethene
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-148.6 - 53.050.2
Density ρg mL-1 2.02 - 2.202.13
Solubility Parameter δMPa1/2 18.5 - 19.619.4
Molar Cohesive Energy EcohJ mol-1 16800 - 1930018800
Glass Transition Temperature TgK 373
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 106.95
Van-der-Waals Volume VvWmL mol-1 33.43
Molar Volume VmmL mol-147.9 - 50.449.2
Density ρg mL-1 2.12 - 2.232.18
Solubility Parameter δMPa1/2 18.7 - 19.319.1
Molar Cohesive Energy EcohJ mol-1 17300 - 1880017900
Glass Transition Temperature TgK 377
Molar Heat Capacity CpJ (mol K)-165 - 6867
Entanglement Molecular Weight Meg mol-16900 - 85007700
Index of Refraction nnone1.61 - 1.621.62