Poly(tert-butylethylene)
CROW logo
Poly(tert-butylethylene)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyalkene (Polyolefin)
COMMON NAMESPoly(tert-butylethylene)
STRUCTURE BASED NAME Poly[1-(tert-butyl)ethylene], Poly[1-(1,1-dimethylethyl)ethylene]
ACRONYMS
CAS #
CurlySMILES C{-}C{n+}(C(C)(C)C)
 

IDENTIFIERS OF MONOMER(S)

CAS # 11069-54-8
COMMON NAMEStert-Butylethylene
SMILES C=CC(C)(C)C
Std. InChI 1S/C6H12/c1-5-6(2,3)4/h5H,1H2,2-4H3
Std. InChIKey PKXHXOTZMFCXSH-UHFFFAOYSA-N
STRUCTURE
tert-Butylethylene
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1
Density ρg mL-1
Solubility Parameter δMPa1/2
Molar Cohesive Energy EcohJ mol-1
Glass Transition Temperature TgK 337
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 84.16
Van-der-Waals Volume VvWmL mol-1 61.68
Molar Volume VmmL mol-193.3 - 101.797.9
Density ρg mL-1 0.83 - 0.900.86
Solubility Parameter δMPa1/2 14.9 - 15.815.4
Molar Cohesive Energy EcohJ mol-1 21600 - 2480023100
Glass Transition Temperature TgK 328 - 348340
Molar Heat Capacity CpJ (mol K)-1138 - 150142
Entanglement Molecular Weight Meg mol-17000 - 97008100
Index of Refraction nnone1.46 - 1.491.48
back to top