Poly(octadecyl acrylate)
CROW logo
Poly(octadecyl acrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyacrylate
COMMON NAMESPoly(octadecyl acrylate), Poly(stearyl acrylate)
STRUCTURE BASED NAME Poly(n-octadecyl propenoate)
ACRONYMS PSA
CAS #  25986-77-0
CurlySMILES C{-}C{n+}(C(=O)OCCCCCCCCCCCCCCCCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 4813-57-4
COMMON NAMES octadecyl acrylate, stearyl acrylate
SMILES CCCCCCCCCCCCCCCCCCCCCCCCCCOC(=O)C=C
Std. InChI InChI=1S/C21H40O2/c1-3-5-6-7-8-9-10-11-12-13-14-15-16-17-18-19-20-23-21(22)4-2/h4H,2-3,5-20H2,1H3
Std. InChIKey FSAJWMJJORKPKS-UHFFFAOYSA-N
STRUCTURE
Stearyl acrylate
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1   
Density ρg mL-1   
Solubility Parameter δMPa1/2 17.7 
Molar Cohesive Energy EcohJ mol-1   
Glass Transition Temperature TgK 308 - 314311
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 324.6
Van-der-Waals Volume VvWmL mol-1 220.7
Molar Volume VmmL mol-1 335 - 352344
Density ρ g mL-1 0.92 - 0.97 0.94
Solubility Parameter δMPa1/2 17.1 - 17.917.4
Molar Cohesive Energy EcohJ mol-1 100000 - 107000104000
Glass Transition Temperature Tg K 273 - 321303
Molar Heat Capacity CpJ (mol K)-1 549 - 592565
Entanglement Molecular Weight Meg mol-1 122000 - 173000147000
Index of Refraction nnone 1.47 - 1.481.48

  Last updated: October 24, 2015