POLYMER CLASS | Polyanhydrides |
COMMON NAMES | Sebacic acid polyanhydride, Poly(sebacic anhydride) |
STRUCTURE BASED NAME | Poly(oxydecanedioyl) |
ACRONYMS | |
CAS # | 26776-29-4 |
CurlySMILES |
CAS # | 123-99-9.108-24-7 |
COMMON NAMES | Sebacic acid + Acetic anhydride |
SMILES | OC(=O)CCCCCCCCC(=O)O.CC(=O)OC(=O)C |
Std. InChI | 1S/C9H16O4/c10-8(11)6-4-2-1-3-5-7-9(12)13/h1-7H2,(H,10,11)(H,12,13).1S/C4H6O3/c1-3(5)7-4(2)6/h1-2H3 |
Std. InChIKey | BDJRBEYXGGNYIS-UHFFFAOYSA-N.WFDIJRYMOXRFFG-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | < 184.2 | |
Density ρ | g mL-1 | > 1.00 | |
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | ||
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 184.24 | |
Van-der-Waals Volume VvW | mL mol-1 | 103.4 | |
Molar Volume Vm | mL mol-1 | 162.4 - 165.4 | 164.3 |
Density ρ | g mL-1 | 1.11 - 1.13 | 1.12 |
Solubility Parameter δ | MPa1/2 | 18.0 - 20.0 | 19.1 |
Molar Cohesive Energy Ecoh | J mol-1 | 52800 - 66300 | 59700 |
Glass Transition Temperature Tg | K | 256 | |
Molar Heat Capacity Cp | J (mol K)-1 | 219 - 234 | 224 |
Entanglement Molecular Weight Me | g mol-1 | 1800 | |
Index of Refraction n | none | 1.49 |