Poly(propyl methacrylate)
CROW logo
Poly(propyl methacrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polymethacrylate
COMMON NAMESPoly(propyl methacrylate)
STRUCTURE BASED NAME Poly(propyl 2-methylpropenoate), Poly[1-(propyloxycarbonyl)-1-methylethylene]
ACRONYMS PPMA
CAS # 25609-74-9
CurlySMILES C{-}C{n+}(C)(C(=O)OCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 2210-28-8
COMMON NAMESPropyl methacrylate
SMILES CCCOC(=O)C(=C)C
Std. InChI 1S/C7H12O2/c1-4-5-9-7(8)6(2)3/h2,4-5H2,1,3H3
Std. InChIKey NHARPDSAXCBDDR-UHFFFAOYSA-N
STRUCTURE
Propyl methacrylate
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1118.7 - 119.3119.0
Density ρg mL-1 1.07 - 1.081.08
Solubility Parameter δMPa1/2 17.9 - 19.618.4
Molar Cohesive Energy EcohJ mol-1 37700 - 4520040100
Glass Transition Temperature TgK 308 - 332319
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone1.48
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 128.17
Van-der-Waals Volume VvWmL mol-1 76.76
Molar Volume VmmL mol-1117.0 - 119.5117.7
Density ρg mL-1 1.07 - 1.101.09
Solubility Parameter δMPa1/2 18.0 - 18.318.1
Molar Cohesive Energy EcohJ mol-1 37600 - 3940038800
Glass Transition Temperature TgK 311 - 329320
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1189 - 200193
Index of Refraction nnone1.48 - 1.491.49