Poly(propyl acrylate)
CROW logo
Poly(propyl acrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyacrylates
COMMON NAMESPoly(propyl acrylate)
STRUCTURE BASED NAME Poly(propyl propenoate)
ACRONYMS
CAS # 24979-82-6
CurlySMILES C{-}C{n+}(C(=O)OCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 925-60-0
COMMON NAMESPropyl acrylate
SMILES CCCOC(=O)C=C
Std. InChI 1S/C6H10O2/c1-3-5-8-6(7)4-2/h4H,2-3,5H2,1H3
Std. InChIKey PNXMTCDJUBJHQJ-UHFFFAOYSA-N
STRUCTURE
Propyl acrylate
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1103.1
Density ρg mL-1 1.11
Solubility Parameter δMPa1/2 18.1 - 19.918.7
Molar Cohesive Energy EcohJ mol-1 33500 - 4060035900
Glass Transition Temperature TgK 228 - 236231
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 114.14
Van-der-Waals Volume VvWmL mol-1 66.48
Molar Volume VmmL mol-1100.8 - 104.4102.2
Density ρg mL-1 1.09 - 1.131.12
Solubility Parameter δMPa1/2 18.3 - 19.318.7
Molar Cohesive Energy EcohJ mol-1 33800 - 3760035700
Glass Transition Temperature TgK 228 - 254 234
Molar Heat Capacity CpJ (mol K)-1167 - 175170
Entanglement Molecular Weight Meg mol-112800 - 1470013800
Index of Refraction nnone1.47 - 1.491.48