POLYMER CLASS | Polymethacrylate |
COMMON NAMES | Poly(2-phenylethyl methacrylate) |
STRUCTURE BASED NAME | Poly(2-Phenylethyl 2-methylpropenoate) |
ACRONYMS | |
CAS # | 28825-60-7 |
CurlySMILES | C{-}C{n+}(C)(C(=O)OCCc1ccccc1) |
CAS # | 222-969-0 |
COMMON NAMES | 2-phenylethyl methacrylate ,2-Phenylethyl 2-methylpropenoate) |
SMILES | CC(=C)C(=O)OCCc1ccccc1 |
Std. InChI | InChI=1S/C12H14O2/c1-10(2)12(13)14-9-8-11-6-4-3-5-7-11/h3-7H,1,8-9H2,2H3 |
Std. InChIKey | ILZXXGLGJZQLTR-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 168.5 | |
Density ρ | g mL-1 | 1.13 | |
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 299 - 329 | |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.55 - 1.56 | 1.55 |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 190.24 | |
Van-der-Waals Volume VvW | mL mol-1 | 112.2 | |
Molar Volume Vm | mL mol-1 | 165 - 170 | 167 |
Density ρ | g mL-1 | 1.12 - 1.15 | 1.14 |
Solubility Parameter δ | MPa1/2 | 19.1 - 19.7 | 19.4 |
Molar Cohesive Energy Ecoh | J mol-1 | 61600 - 64700 | 63100 |
Glass Transition Temperature Tg | K | 352 | |
Molar Heat Capacity Cp | J (mol K)-1 | 245 - 258 | 250 |
Entanglement Molecular Weight Me | g mol-1 | 43000 - 57000 | 50000 |
Index of Refraction n | none | 1.56 - 1.57 | 1.56 |
Last updated: December 23, 2015