POLYMER CLASS | Polyvinylether |
COMMON NAMES | Poly(octyl vinyl ether), Poly(vinyl octyl ether) |
STRUCTURE BASED NAME | Poly(octyloxyethylene) |
ACRONYMS | |
CAS # | |
CurlySMILES | C{-}C{n+}(OCCCCCCCC) |
CAS # | 213-204-1 |
COMMON NAMES | Octyl vinyl ether, 1-(Vinyloxy)octane, |
SMILES | CCCCCCCCOC=C |
Std. InChI | 1S/C10H20O/c1-3-5-6-7-8-9-10-11-4-2/h4H,2-3,5-10H2,1H3 |
Std. InChIKey | XXCVIFJHBFNFBO-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 171 | |
Density ρ | g mL-1 | 0.91 | |
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 193 - 194 | 193 |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.46 |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 157.3 | |
Van-der-Waals Volume VvW | mL mol-1 | 104.8 | |
Molar Volume Vm | mL mol-1 | 162 - 174 | 170 |
Density ρ | g mL-1 | 0.90 - 0.96 | 0.92 |
Solubility Parameter δ | MPa1/2 | 16.8 - 17.7 | 17.1 |
Molar Cohesive Energy Ecoh | J mol-1 | 48800 - 50700 | 49800 |
Glass Transition Temperature Tg | K | 184 - 211 | 196 |
Molar Heat Capacity Cp | J (mol K)-1 | 322 - 342 | 332 |
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.47 - 1.48 | 1.47 |