POLYMER CLASS | Polymethacrylate |
COMMON NAMES | Poly(octyl methacrylate) |
STRUCTURE BASED NAME | Poly(octyl 2-methylpropenoate), Poly[1-(octyloxycarbonyl)-1-methylethylene] |
ACRONYMS | |
CAS # | 25087-18-7 |
CurlySMILES | C{-}C{n+}(C)(C(=O)OCCCCCCCC) |
CAS # | 2157-01-9 |
COMMON NAMES | Octyl methacrylate, Octyl 2-methyl-2-propenoate |
SMILES | CCCCCCCCOC(=O)C(=C)C |
Std. InChI | InChI=1S/C12H22O2/c1-4-5-6-7-8-9-10-14-12(13)11(2)3/h2,4-10H2,1,3H3 |
Std. InChIKey | NZIDBRBFGPQCRY-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 204.2 | |
Density ρ | g mL-1 | 0.97 | |
Solubility Parameter δ | MPa1/2 | 17.1 - 17.2 | 17.1 |
Molar Cohesive Energy Ecoh | J mol-1 | 59700 - 60400 | 60100 |
Glass Transition Temperature Tg | K | 203 - 253 | 228 |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | 47100 - 86700 | 67000 |
Index of Refraction n | none |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 198.3 | |
Van-der-Waals Volume VvW | mL mol-1 | 128.2 | |
Molar Volume Vm | mL mol-1 | 194.8 - 202 | 198.4 |
Density ρ | g mL-1 | 0.98 - 1.02 | 1.0 |
Solubility Parameter δ | MPa1/2 | 17.4 - 17.9 | 17.6 |
Molar Cohesive Energy Ecoh | J mol-1 | 59800 - 62600 | 61500 |
Glass Transition Temperature Tg | K | 234 | |
Molar Heat Capacity Cp | J (mol K)-1 | 382 - 402 | 392 |
Entanglement Molecular Weight Me | g mol-1 | 44000 - 48100 | 46100 |
Index of Refraction n | none | 1.48 - 1.49 | 1.48 |
Last updated: October 18, 2015