Poly(octyl cyanoacrylate)
CROW logo
Poly(octyl cyanoacrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polycyanoacrylates
COMMON NAMESPoly(octyl cyanoacrylate)
STRUCTURE BASED NAME Poly(octyl 2-cyanopropenoate), Poly(octyl α-cyanoacrylate)
ACRONYMS
CAS #  
CurlySMILES C{-}C{n+}(C#N)(C(=O)OCCCCCCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 229-748-8
COMMON NAMESOctyl 2-cyanoacrylate
SMILES CCCCCCCCOC(=O)C(=C)C#N
Std. InChI 1S/C12H19NO2/c1-3-4-5-6-7-8-9-15-12(14)11(2)10-13/h2-9H2,1H3
Std. InChIKey RPQUGMLCZLGZTG-UHFFFAOYSA-N
STRUCTURE
Poly(octyl cyanoacrylate)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1
Density ρg mL-1
Solubility Parameter δMPa1/2   
Molar Cohesive Energy EcohJ mol-1
Glass Transition Temperature TgK 313- 331322
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 209.29
Van-der-Waals Volume VvWmL mol-1 129.8
Molar Volume VmmL mol-1 194 - 196195.5
Density ρg mL-1 1.07 - 1.081.07
Solubility Parameter δMPa1/2 19.9 - 20.720.1
Molar Cohesive Energy Ecoh J mol-1 78000 - 8300079000
Glass Transition Temperature TgK 212 - 232, 308308
Molar Heat Capacity CpJ (mol K)-1 321 (l)
397 (s)
 
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone 1.49 - 1.501.49