POLYMER CLASS | Polyalkene (Polyolefin) |
COMMON NAMES | Poly(hexylethylene) |
STRUCTURE BASED NAME | Poly(1-octene) |
ACRONYMS | |
CAS # | |
CurlySMILES | C{-}C{n+}(CCCCCC) |
CAS # | 111-66-0 |
COMMON NAMES | 1-Octene |
SMILES | CCCCCCC=C |
Std. InChI | 1S/C8H16/c1-3-5-7-8-6-4-2/h3H,1,4-8H2,2H3 |
Std. InChIKey | KWKAKUADMBZCLK-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 1291 | |
Density ρ | g mL-1 | 0.871 | |
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 208 - 228 | 218 |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 112.2 | |
Van-der-Waals Volume VvW | mL mol-1 | 82.2 | |
Molar Volume Vm | mL mol-1 | 124 - 134 | 130 |
Density ρ | g mL-1 | 0.84 - 0.90 | 0.86 |
Solubility Parameter δ | MPa1/2 | 16.0 - 16.8 | 16.4 |
Molar Cohesive Energy Ecoh | J mol-1 | 34400 - 35400 | 35000 |
Glass Transition Temperature Tg | K | 203 - 225 | 218 |
Molar Heat Capacity Cp | J (mol K)-1 | 234 - 249 | 240 |
Entanglement Molecular Weight Me | g mol-1 | 13900 | |
Index of Refraction n | none | 1.47 - 1.48 | 1.47 |
Last updated: April 23, 2016