POLYMER CLASS | Polyacrylamide |
COMMON NAMES | Poly(N-tert-butyl acrylamide), Poly[N-(2-methyl-2-propanyl)acrylamide] |
STRUCTURE BASED NAME | Poly[(N-tert-butylaminocarbonyl)ethylene] |
ACRONYMS | |
CAS # | |
CurlySMILES | C{-}C{n+}(C(=O)NC(C)(C)C) |
CAS # | 107-58-4 |
COMMON NAMES | N-tert-Butyl acrylamide |
SMILES | C=CC(=O)NC(C)(C)C |
Std. InChI | 1S/C7H13NO/c1-5-6(9)8-7(2,3)4/h5H,1H2,2-4H3,(H,8,9) |
Std. InChIKey | XFHJDMUEHUHAJW-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 123.0 | |
Density ρ | g mL-1 | 1.03 | |
Solubility Parameter δ | MPa1/2 | 18.4 - 26.7 | 23.0 |
Molar Cohesive Energy Ecoh | J mol-1 | 41600 - 87700 | 65200 |
Glass Transition Temperature Tg | K | 401 | |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 127.19 | |
Van-der-Waals Volume VvW | mL mol-1 | 79.10 | |
Molar Volume Vm | mL mol-1 | 121.6 - 123.7 | 123.0 |
Density ρ | g mL-1 | 1.03 - 1.05 | 1.03 |
Solubility Parameter δ | MPa1/2 | 22.4 - 22.5 | 22.4 |
Molar Cohesive Energy Ecoh | J mol-1 | 61900 - 62300 | 61900 |
Glass Transition Temperature Tg | K | 402 - 433 | 420 |
Molar Heat Capacity Cp | J (mol K)-1 | 184 - 200 | 190 |
Entanglement Molecular Weight Me | g mol-1 | 28100 - 28400 | 28200 |
Index of Refraction n | none | 1.49 - 1.52 | 1.50 |