PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | ||
Density ρ | g mL-1 | ||
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 390 | |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 127.19 | |
Van-der-Waals Volume VvW | mL mol-1 | 79.10 | |
Molar Volume Vm | mL mol-1 | 121.6 - 125.1 | 123.7 |
Density ρ | g mL-1 | 1.02 - 1.05 | 1.03 |
Solubility Parameter δ | MPa1/2 | 22.5 - 22.7 | 22.6 |
Molar Cohesive Energy Ecoh | J mol-1 | 63200 - 63900 | 63200 |
Glass Transition Temperature Tg | K | 357 - 393 | 393 |
Molar Heat Capacity Cp | J (mol K)-1 | 189 - 200 | 194 |
Entanglement Molecular Weight Me | g mol-1 | 28000 - 29000 | 28500 |
Index of Refraction n | none | 1.48 - 1.51 | 1.49 |