POLYMER CLASS | Polyacrylamide |
COMMON NAMES | Poly(N-phenylacrylamide) |
STRUCTURE BASED NAME | Poly[(N-phenylaminocarbonyl)ethylene] |
ACRONYMS | |
CAS # | |
CurlySMILES | C{-}C{n+}(C(=O)Nc1ccccc1) |
CAS # | 2210-24-4 |
COMMON NAMES | N-Phenylacrylamide |
SMILES | C=CC(=O)Nc1ccccc1 |
Std. InChI | 1S/C9H9NO/c1-2-9(11)10-8-6-4-3-5-7-8/h2-7H,1H2,(H,10,11) |
Std. InChIKey | BPCNEKWROYSOLT-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 127.0 - 130.0 | 128.5 |
Density ρ | g mL-1 | 1.13 - 1.16 | 1.15 |
Solubility Parameter δ | MPa1/2 | 21.4 - 28.5 | 24.9 |
Molar Cohesive Energy Ecoh | J mol-1 | 56800 - 100700 | 79800 |
Glass Transition Temperature Tg | K | ||
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 147.18 | |
Van-der-Waals Volume VvW | mL mol-1 | 83.71 | |
Molar Volume Vm | mL mol-1 | 120.7 - 127.9 | 124.0 |
Density ρ | g mL-1 | 1.15 - 1.22 | 1.19 |
Solubility Parameter δ | MPa1/2 | 25.5 - 26.2 | 25.9 |
Molar Cohesive Energy Ecoh | J mol-1 | 80700 - 82900 | 82900 |
Glass Transition Temperature Tg | K | (498) | |
Molar Heat Capacity Cp | J (mol K)-1 | 171 - 183 | 177 |
Entanglement Molecular Weight Me | g mol-1 | 42000 - 50000 | 47000 |
Index of Refraction n | none | 1.60 - 1.63 | 1.61 |