POLYMER CLASS | Polyacrylamide |
COMMON NAMES | Poly(N-octyl acrylamide) |
STRUCTURE BASED NAME | Poly[(N-octylaminocarbonyl)ethylene] |
ACRONYMS | |
CAS # | |
CurlySMILES | C{-}C{n+}(C(=O)NCCCCCCCC) |
CAS # | 10124-68-2 |
COMMON NAMES | |
SMILES | CCCCCCCCNC(=O)C=C |
Std. InChI | 1S/C11H21NO/c1-3-5-6-7-8-9-10-12-11(13)4-2/h4H,2-3,5-10H2,1H3,(H,12,13) |
Std. InChIKey | AWGZKFQMWZYCHF-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 183.5 | |
Density ρ | g mL-1 | 1.00 | |
Solubility Parameter δ | MPa1/2 | 19.0 - 23.8 | 21.8 |
Molar Cohesive Energy Ecoh | J mol-1 | 67600 - 106100 | 87000 |
Glass Transition Temperature Tg | K | 220 | |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 183.30 | |
Van-der-Waals Volume VvW | mL mol-1 | 120.22 | |
Molar Volume Vm | mL mol-1 | 183.8 - 189.3 | 187.4 |
Density ρ | g mL-1 | 0.97 - 1.00 | 0.98 |
Solubility Parameter δ | MPa1/2 | 20.9 - 21.0 | 20.9 |
Molar Cohesive Energy Ecoh | J mol-1 | 82200 - 82900 | 82200 |
Glass Transition Temperature Tg | K | 228 | 228 |
Molar Heat Capacity Cp | J (mol K)-1 | 373 - 392 | 389 |
Entanglement Molecular Weight Me | g mol-1 | 49000 - 59500 | 57000 |
Index of Refraction n | none | 1.48 - 1.49 | 1.49 |