Poly(N-benzyl methacrylamide)
CROW logo
Poly(N-benzyl methacrylamide)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polymethacrylamide
COMMON NAMESPoly(N-benzyl methacrylamide)
STRUCTURE BASED NAME Poly(2-methyl-N-(phenylmethyl)-2-propenamide)
ACRONYMS
CAS #
CurlySMILES C{-}C{n+}(C)(C(=O)NCc1ccccc1)
 

IDENTIFIERS OF MONOMER(S)

CAS # 3219-55-4
COMMON NAMESN-Benzyl-2-methylacrylamide
SMILES O=C(C(=C)C)NCc1ccccc1
Std. InChI 1S/C11H13NO/c1-9(2)11(13)12-8-10-6-4-3-5-7-10/h3-7H,1,8H2,2H3,(H,12,13)
Std. InChIKey CEBFLGHPYLIZSC-UHFFFAOYSA-N
STRUCTURE
N-Benzyl-2-methylacrylamide
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1151.0 - 160.0155.5
Density ρg mL-1 1.10 - 1.111.13
Solubility Parameter δMPa1/2 20.0 - 25.022.5
Molar Cohesive Energy EcohJ mol-1 62200 - 9720078700
Glass Transition Temperature TgK
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone1.47 - 1.601.60
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 175.23
Van-der-Waals Volume VvWmL mol-1 104.27
Molar Volume VmmL mol-1152.3 - 159.0155.6
Density ρg mL-1 1.10 - 1.151.13
Solubility Parameter δMPa1/2 23.6 - 24.123.8
Molar Cohesive Energy EcohJ mol-1 86300 - 8820088200
Glass Transition Temperature TgK 495
Molar Heat Capacity CpJ (mol K)-1220 - 233226
Entanglement Molecular Weight Meg mol-156000 - 7000063000
Index of Refraction nnone1.58 - 1.611.59
back to top