PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 112 | |
Density ρ | g mL-1 | 1.14 | |
Solubility Parameter δ | MPa1/2 | 22.6 - 29.5 | 26.8 |
Molar Cohesive Energy Ecoh | J mol-1 | 52900 - 90200 | 74300 |
Glass Transition Temperature Tg | K | ||
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 127.14 | |
Van-der-Waals Volume VvW | mL mol-1 | 69.77 | |
Molar Volume Vm | mL mol-1 | 103.6 - 107.8 | 105.7 |
Density ρ | g mL-1 | 1.18 - 1.28 | 1.23 |
Solubility Parameter δ | MPa1/2 | 27.2 - 28.3 | 27.7 |
Molar Cohesive Energy Ecoh | J mol-1 | 76400 - 83000 | 79700 |
Glass Transition Temperature Tg | K | 445 | |
Molar Heat Capacity Cp | J (mol K)-1 | 161 - 175 | 168 |
Entanglement Molecular Weight Me | g mol-1 | 26600 - 36600 | 31600 |