POLYMER CLASS | Polyvinylether |
COMMON NAMES | Poly(methyl vinyl ether), Gantrez®, Lutonal® M40 |
STRUCTURE BASED NAME | Poly(methoxyethylene) |
ACRONYMS | PVME |
CAS # | 9003-09-2 |
CurlySMILES | C{-}C{n+}(OC) |
CAS # | 100-39-0 |
COMMON NAMES | Methyl Vinyl Ether |
SMILES | COC=C |
Std. InChI | 1S/C3H6O/c1-3-4-2/h3H,1H2,2H3 |
Std. InChIKey | XJRBAMWJDBPFIM-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 54.9 - 56.4 | 55.6 |
Density ρ | g mL-1 | 1.03 - 1.06 | 1.05 |
Solubility Parameter δ | MPa1/2 | 16.7 - 19.7 | 18.3 |
Molar Cohesive Energy Ecoh | J mol-1 | 16400 - 22800 | 18600 |
Glass Transition Temperature Tg | K | 228 - 260 | 245 |
Molar Heat Capacity Cp | J (mol K)-1 | 113 | |
Entanglement Molecular Weight Me | g mol-1 | 5100 - 6450 | 5800 |
Index of Refraction n | none | 1.46 - 1.47 | 1.46 |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 58.08 | |
Van-der-Waals Volume VvW | mL mol-1 | 32.81 | |
Molar Volume Vm | mL mol-1 | 57.7 - 59.8 | 58.7 |
Density ρ | g mL-1 | 0.97 - 1.03 | 1.01 |
Solubility Parameter δ | MPa1/2 | 17.0 - 18.5 | 17.6 |
Molar Cohesive Energy Ecoh | J mol-1 | 16900 - 18400 | 18100 |
Glass Transition Temperature Tg | K | 255 - 257 | 256 |
Molar Heat Capacity Cp | J (mol K)-1 | 117 - 124 | 120 |
Entanglement Molecular Weight Me | g mol-1 | 3800 - 6400 | 5100 |
Index of Refraction n | none | 1.46 - 1.47 | 1.46 |