Poly(isopropyl vinyl ether)
CROW logo
Poly(isopropyl vinyl ether)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyvinylether
COMMON NAMESPoly(isopropyl vinyl ether), Poly(vinyl isopropyl ether), Lutonal® I60
STRUCTURE BASED NAME Poly(isopropoxyethylene)
ACRONYMS
CAS # 25585-49-3
CurlySMILES C{-}C{n+}(OC(C)C)
 

IDENTIFIERS OF MONOMER(S)

CAS # 926-65-8
COMMON NAMESVinyl isopropyl ether
SMILES C=COC(C)C
Std. InChI 1S/C5H10O/c1-4-6-5(2)3/h4-5H,1H2,2-3H3
Std. InChIKey GNUGVECARVKIPH-UHFFFAOYSA-N
STRUCTURE
Vinyl isopropyl ether
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-193.2
Density ρg mL-1 0.92
Solubility Parameter δMPa1/2 16.4 - 19.317.9
Molar Cohesive Energy EcohJ mol-1 25000 - 34600 29900
Glass Transition Temperature TgK 261 - 270270
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 86.13
Van-der-Waals Volume VvWmL mol-1 53.37
Molar Volume VmmL mol-192.7 - 93.292.9
Density ρg mL-1 0.92 - 0.930.93
Solubility Parameter δMPa1/2 16.2 - 17.416.7
Molar Cohesive Energy EcohJ mol-1 24400 - 2660025800
Glass Transition Temperature TgK 253 - 281267
Molar Heat Capacity CpJ (mol K)-1175 - 183178
Entanglement Molecular Weight Meg mol-16700 - 102009100
Index of Refraction nnone1.45 - 1.471.45