POLYMER CLASS | Polyvinylether |
COMMON NAMES | Polyhexyl vinyl ether.html, Poly(vinyl n-hexyl ether) |
STRUCTURE BASED NAME | Poly(hexyloxyethylene) |
ACRONYMS | |
CAS # | |
CurlySMILES | C{-}C{n+}(OCCCCCC) |
CAS # | |
COMMON NAMES | Hexyl vinyl ether |
SMILES | CCCCCCOC=C |
Std. InChI | 1S/C8H16O/c1-3-5-6-7-8-9-4-2/h4H,2-3,5-8H2,1H3 |
Std. InChIKey | YAOJJEJGPZRYJF-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | 138.5 | |
Density ρ | g mL-1 | 0.93 | |
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 196 - 199 | 198 |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.46 |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 128.22 | |
Van-der-Waals Volume VvW | mL mol-1 | 84.21 | |
Molar Volume Vm | mL mol-1 | 131 - 142 | 137.5 |
Density ρ | g mL-1 | 0.91 - 0.98 | 0.93 |
Solubility Parameter δ | MPa1/2 | 16.8 - 17.8 | 17.2 |
Molar Cohesive Energy Ecoh | J mol-1 | 39800 - 41400 | 40600 |
Glass Transition Temperature Tg | K | 193- 210 | 201 |
Molar Heat Capacity Cp | J (mol K)-1 | 264 - 279 | 271 (l) |
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.47 | 1.47 |