Poly(hexyl methacrylate)
CROW logo
Poly(hexyl methacrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polymethacrylate
COMMON NAMESPoly(hexyl methacrylate)
STRUCTURE BASED NAME Poly(hexyl 2-methylpropenoate), Poly[1-(hexyloxycarbonyl)-1-methylethylene]
ACRONYMS
CAS # 25087-17-6
CurlySMILES C{-}C{n+}(C)(C(=O)OCCCCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 142-09-6
COMMON NAMESHexyl methacylate
SMILES CCCCCCOC(=O)C(=C)C
Std. InChI 1S/C10H18O2/c1-4-5-6-7-8-12-10(11)9(2)3/h2,4-8H2,1,3H3
Std. InChIKey LNCPIMCVTKXXOY-UHFFFAOYSA-N
STRUCTURE
Hexyl methacrylate
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1168.8 - 169.1169.0
Density ρg mL-1 1.011.01
Solubility Parameter δMPa1/2 17.2 - 17.617.4
Molar Cohesive Energy EcohJ mol-1 50000 - 5230051200
Glass Transition Temperature TgK 256 - 274266
Molar Heat Capacity CpJ (mol K)-1324
Entanglement Molecular Weight Meg mol-133100 - 3380033500
Index of Refraction nnone1.48
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 170.25
Van-der-Waals Volume VvWmL mol-1 107.60
Molar Volume VmmL mol-1163.7 - 169.0166.1
Density ρg mL-1 1.01 - 1.041.03
Solubility Parameter δMPa1/2 17.5 - 18.017.8
Molar Cohesive Energy EcohJ mol-1 50900 - 5330052400
Glass Transition Temperature TgK 264
Molar Heat Capacity CpJ (mol K)-1324 - 338332
Entanglement Molecular Weight Meg mol-132200 - 3300032600
Index of Refraction nnone1.47 - 1.491.48