Poly(ethyleneketone)
CROW logo
Poly(ethyleneketone)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyketone
COMMON NAMESPoly(ethyleneketone), Carilon®, Poketone™, Akrotek® PK
STRUCTURE BASED NAME Poly(1-oxotrimethylene)
ACRONYMS PEK
CAS #
CurlySMILES C{-}CC{n+}(=O)
 

IDENTIFIERS OF MONOMER(S)

CAS # 74-85-1.630-08-0
COMMON NAMESEthylene, Carbon monoxide
SMILES C=C.[C-]#[O+]
Std. InChI 1S/C2H4/c1-2/h1-2H2.1S/CH2O/c1-2/h1H2
Std. InChIKey VGGSQFUCUMXWEO-UHFFFAOYSA-N.WSFSSNUMVMOOMR-UHFFFAOYSA-N
STRUCTURE
Poly(ethyleneketone)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-145.2
Density ρg mL-1 1.24
Solubility Parameter δMPa1/2
Molar Cohesive Energy EcohJ mol-1
Glass Transition Temperature TgK 291
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 56.06
Van-der-Waals Volume VvWmL mol-1 31.79
Molar Volume VmmL mol-143.8 - 48.446.1
Density ρg mL-1 1.16 - 1.281.22
Solubility Parameter δMPa1/2 22.2 - 26.524.5
Molar Cohesive Energy EcohJ mol-1 23900 - 3250027600
Glass Transition Temperature TgK 277 - 303290
Molar Heat Capacity CpJ (mol K)-174 - 82
114 - 117
76 (s)
115 (l,r)
Entanglement Molecular Weight Meg mol-13800 - 56004700
Index of Refraction n none 1.48 - 1.54 1.52

  Last updated: July 18, 2016