Poly(ethyl acrylate)
CROW logo
Poly(ethyl acrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyacrylates
COMMON NAMESPoly(ethyl acrylate)
STRUCTURE BASED NAME Poly(ethyl propenoate), Poly[1-(ethoxycarbonyl)ethylene]
ACRONYMS
CAS # 9003-32-1
CurlySMILES C{-}C{n+}(C(=O)OCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 140-88-5
COMMON NAMESEthyl acrylate
SMILES CCOC(=O)C=C
Std. InChI 1S/C5H8O2/c1-3-5(6)7-4-2/h3H,1,4H2,2H3
Std. InChIKey JIGUQPWFLRLWPJ-UHFFFAOYSA-N
STRUCTURE
Ethylacrylate
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-189.4
Density ρg mL-1 1.12
Solubility Parameter δMPa1/2 18.5 - 19.219.1
Molar Cohesive Energy EcohJ mol-1 30600 - 3300032800
Glass Transition Temperature TgK 248 - 251250
Molar Heat Capacity CpJ (mol K)-1179 - 182180
Entanglement Molecular Weight Meg mol-17800 - 86008200
Index of Refraction nnone1.46 - 1.471.47
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 100.12
Van-der-Waals Volume VvWmL mol-1 56.20
Molar Volume VmmL mol-184.4 - 87.986.1
Density ρg mL-1 1.14 - 1.191.16
Solubility Parameter δMPa1/2 18.7 - 19.619.1
Molar Cohesive Energy EcohJ mol-1 29400 - 3310031300
Glass Transition Temperature TgK 225 - 260254
Molar Heat Capacity CpJ (mol K)-1183 - 190185
Entanglement Molecular Weight Meg mol-19250 - 96009400
Index of Refraction nnone1.46 - 1.491.47