Poly(ether ketone)
CROW logo
Poly(ether ketone)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyetherketone
COMMON NAMESPoly(ether ketone), Poly(4,4'-dichlorobenzophenone), Victrex® PEK, Ultrapek®
STRUCTURE BASED NAME Poly(oxy-1,4-phenylenecarbonyl-1,4-phenylene)
ACRONYMS PEK
CAS # 27380-27-4
CurlySMILES O{-}c1ccc(cc1)C(=O)c1ccc{n+}(cc1)
 

IDENTIFIERS OF MONOMER(S)

CAS # 1332-57-6.6284-79-3
COMMON NAMESSodium carbonate + 4,4'-Dichlorobenzophenone
SMILES [O-]C(=O)[O-].[Na+].[Na+].O=C(c1ccc(cc1)Cl)c1ccc(cc1)Cl
Std. InChI 1S/CH2O3.2Na/c2-1(3)4;;/h(H2,2,3,4);;/q;2*+1/p-2.1S/C13H8Cl2O/c14-11-5-1-9(2-6-11)13(16)10-3-7-12(15)8-4-10/h1-8H
Std. InChIKey CDBYLPFSWZWCQE-UHFFFAOYSA-L.OKISUZLXOYGIFP-UHFFFAOYSA-N
STRUCTURE
Poly(ether ketone)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1155.2
Density ρg mL-1 1.27 (amorphous)
1.43 (crystalline)
Solubility Parameter δMPa1/2 22.9 - 23.123.0
Molar Cohesive Energy EcohJ mol-1 80900 - 8250081700
Glass Transition Temperature TgK 425 - 436431
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 196.21
Van-der-Waals Volume VvWmL mol-1 104.35
Molar Volume VmmL mol-1154.4 - 160.8157.7
Density ρg mL-1 1.22 - 1.271.24
Solubility Parameter δMPa1/2 21.7 - 23.922.6
Molar Cohesive Energy EcohJ mol-1 76000 - 8840080700
Glass Transition Temperature TgK 437
Molar Heat Capacity CpJ (mol K)-1197 - 212202
Entanglement Molecular Weight Meg mol-11300 - 25001750
Index of Refraction nnone1.60 - 1.721.66