Poly(epichlorohydrin)
CROW logo
Poly(epichlorohydrin)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyglycol
COMMON NAMESPoly(epichlorohydrin)
STRUCTURE BASED NAME Poly(3-Chloro-1,2-oxypropylene), Poly[oxy(1-(chloromethyl)ethylene)], Poly(chloromethyl)ethylene oxide)
ACRONYMS
CAS # 24969-06-0
CurlySMILES O{-}CC{n+}(CCl)
 

IDENTIFIERS OF MONOMER(S)

CAS # 106-89-8
COMMON NAMESEpichlorohydrin
SMILES ClCC1CO1
Std. InChI 1S/C3H5ClO/c4-1-3-2-5-3/h3H,1-2H2
Std. InChIKey BRLQWZUYTZBJKN-UHFFFAOYSA-N
STRUCTURE
Poly(epichlorohydrin)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-168.0 - 69.768.9
Density ρg mL-1 1.33 - 1.361.34
Solubility Parameter δMPa1/2 18.6 - 20.119.7
Molar Cohesive Energy EcohJ mol-1 23900 - 2790026800
Glass Transition Temperature TgK 251 - 256253
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 92.52
Van-der-Waals Volume VvWmL mol-1 41.07
Molar Volume VmmL mol-166.6 - 72.169.0
Density ρg mL-1 1.28 - 1.391.34
Solubility Parameter δMPa1/2 19.0 - 20.5 19.9
Molar Cohesive Energy EcohJ mol-1 26100 - 2810027200
Glass Transition Temperature TgK 256
Molar Heat Capacity CpJ (mol K)-1145 - 157150
Entanglement Molecular Weight Meg mol-14500 - 85006300
Index of Refraction nnone1.50 - 1.521.51

  Last updated: July 21, 2019