Poly[di(n-propyl) itaconate]
CROW logo

       
Poly[di(n-propyl) itaconate]
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyitaconate
COMMON NAMESPoly[di(n-propyl) itaconate]
STRUCTURE BASED NAME Poly[di(n-propyl)-2-methylidene butandioate], Poly[di(n-propyl)-2-methylenesuccinate]
ACRONYMS
CAS #
CurlySMILES C{-}(C(=O)OCCC)(CC(=O)OCCC)C{n+}
 

IDENTIFIERS OF MONOMER(S)

CAS # 13401-95-1
COMMON NAMESDi(n-propyl) itaconate
SMILES CCCOC(=O)CC(=C)C(=O)OCCC
Std. InChI 1S/C11H18O4/c1-4-6-14-10(12)8-9(3)11(13)15-7-5-2/h3-8H2,1-2H3
Std. InChIKey DFQSWFGKYUFIFW-UHFFFAOYSA-N
STRUCTURE
Di-n-propylitaconate
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1
Density ρg mL-1
Solubility Parameter δMPa1/2 18.3 - 19.018.6
Molar Cohesive Energy EcohJ mol-1 62500 - 6740064600
Glass Transition Temperature TgK 304 - 307306
Molar Heat Capacity CpJ (mol K)-1328 (s)
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 214.26
Van-der-Waals Volume VvWmL mol-1 122.68
Molar Volume VmmL mol-1183.8 - 188.9186.7
Density ρg mL-1 1.13 - 1.171.15
Solubility Parameter δMPa1/2 18.6 - 19.319.0
Molar Cohesive Energy EcohJ mol-1 63400 - 7000067200
Glass Transition Temperature TgK 303303
Molar Heat Capacity CpJ (mol K)-1310 - 324
389 - 409
318 (s)
398 (l,r)
Entanglement Molecular Weight Meg mol-152000 - 5500053500
Index of Refraction nnone1.47 - 1.491.48
back to top