Poly(dimethyl fumarate)
CROW logo
Poly(dimethyl fumarate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyfumarate
COMMON NAMESPoly(dimethyl fumarate)
STRUCTURE BASED NAME Poly(dimethyl-but-2-enedioate)
ACRONYMS
CAS #
CurlySMILES C{-}(C(=O)OC)C{n+}(C(=O)OC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 624-49-7
COMMON NAMES
SMILES COC(=O)/C=C/C(=O)OC
Std. InChI 1S/C6H8O4/c1-9-5(7)3-4-6(8)10-2/h3-4H,1-2H3/b4-3+
Std. InChIKey LDCRTTXIJACKKU-ONEGZZNKSA-N
STRUCTURE
Poly(dimethyl fumarate)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1115.5
Density ρg mL-1 1.25
Solubility Parameter δMPa1/2 19.6 - 20.119.9
Molar Cohesive Energy EcohJ mol-1 44400 - 4670045600
Glass Transition Temperature TgK 367 - 378373
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 144.13
Van-der-Waals Volume VvWmL mol-1 71.28
Molar Volume VmmL mol-1103.4 - 109.9107.6
Density ρg mL-1 1.31 - 1.391.34
Solubility Parameter δMPa1/2 20.0 - 20.920.4
Molar Cohesive Energy EcohJ mol-1 41500 - 4800044800
Glass Transition Temperature TgK 368 - 379374
Molar Heat Capacity CpJ (mol K)-1172 - 200185
Entanglement Molecular Weight Meg mol-113000 - 2000016500
Index of Refraction nnone1.46 - 1.491.48