Poly(dibutylfumarate)
CROW logo
Poly(dibutyl fumarate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyfumarate
COMMON NAMESPoly(dibutyl fumarate)
STRUCTURE BASED NAME Poly(butyl-2-butenedioate)
ACRONYMS
CAS #
CurlySMILES C{-}(C(=O)OCCCC)C{n+}(C(=O)OCCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 105-75-9
COMMON NAMES n-Butyl fumarate, Dibutyl-(2E)-2-butenedioate
SMILES CCCCOC(=O)/C=C/C(=O)OCCCC
Std. InChI 1S/C12H20O4/c1-3-5-9-15-11(13)7-8-12(14)16-10-6-4-2/h7-8H,3-6,9-10H2,1-2H3/b8-7+
Std. InChIKey JBSLOWBPDRZSMB-BQYQJAHWSA-N
STRUCTURE
Poly(dibutyl fumarate)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1  
Density ρg mL-1  
Solubility Parameter δMPa1/2   
Molar Cohesive Energy EcohJ mol-1   
Glass Transition Temperature TgK   
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 228.29
Van-der-Waals Volume VvW mL mol-1 133
Molar Volume VmmL mol-1 203 - 209205
Density ρg mL-1 1.09 - 1.131.12
Solubility Parameter δMPa1/2 18.3 - 19.318.7
Molar Cohesive Energy EcohJ mol-1 68000 - 7500071500
Glass Transition Temperature TgK 228 - 274242
Molar Heat Capacity CpJ (mol K)-1 333 - 353 (s)
422 - 438 (l)
343 (s)
430 (l)
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone 1.47 - 1.491.48

  Last updated: January 15, 2017