Poly(n-decyl methacrylate)
CROW logo
Poly(decyl methacrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polymethacrylate
COMMON NAMESPoly(n-decyl methacrylate)
STRUCTURE BASED NAME Poly(n-decyl 2-methylpropenoate)
ACRONYMS
CAS #  
CurlySMILES C{-}C{n+}(C)(C(=O)OCCCCCCCCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 221-657-1
COMMON NAMESn-Decyl methacrylate
SMILES CCCCCCCCCCOC(=O)C(=C)C
Std. InChI InChI=1S/C14H26O2/c1-4-5-6-7-8-9-10-11-12-16-14(15)13(2)3/h2,4-12H2,1,3H3
Std. InChIKey GTBGXKPAKVYEKJ-UHFFFAOYSA-N
STRUCTURE
Poly(decyl methacrylate)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1 238 - 242240
Density ρg mL-1 0.94 - 0.950.95
Solubility Parameter δMPa1/2   
Molar Cohesive Energy EcohJ mol-1   
Glass Transition Temperature TgK 203 - 218211
Molar Heat Capacity CpJ (mol K)-1   
Entanglement Molecular Weight Meg mol-1 60900 - 6130061100
Index of Refraction nnone  
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 226.4
Van-der-Waals Volume VvWmL mol-1 148.7
Molar Volume VmmL mol-1 231 - 235233
Density ρg mL-1 0.96 - 0.980.97
Solubility Parameter δ MPa1/2 17.2 - 17.8 17.4
Molar Cohesive Energy EcohJ mol-1 68600 - 7190070900
Glass Transition Temperature TgK 200 - 238219
Molar Heat Capacity CpJ (mol K)-1 441 - 466452.5
Entanglement Molecular Weight Meg mol-1 57700 - 6730062500
Index of Refraction nnone 1.48 - 1.491.48