Polydecene
CROW logo
Poly(1-decene)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyalkene (Polyolefin)
COMMON NAMESPoly(octylethylene)
STRUCTURE BASED NAME Poly(1-decene)
ACRONYMS  
CAS # 25511-67-5
CurlySMILES C{-}(CCCCCCCC)C{n+}
 

IDENTIFIERS OF MONOMER(S)

CAS # 872-05-9
COMMON NAMES1-decene
SMILES CCCCCCCCC=C
Std. InChI 1S/C10H20/c1-3-5-7-9-10-8-6-4-2/h3H,1,4-10H2,2H3
Std. InChIKey AFFLGGQVNFXPEV-UHFFFAOYSA-N
STRUCTURE
1-Decene
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-11601 - 162 
Density ρg mL-1 0.86 - 0.871 
Solubility Parameter δMPa1/2   
Molar Cohesive Energy Ecoh J mol-1
Glass Transition Temperature TgK 232 
Molar Heat Capacity CpJ (mol K)-1   
Entanglement Molecular Weight Meg mol-1 23000 
Index of Refraction nnone 1.47 
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unit g mol-1 140.27
Van-der-Waals Volume VvWmL mol-1 102.8
Molar Volume VmmL mol-1 155.5 - 167162
Density ρg mL-1 0.84 - 0.900.86
Solubility Parameter δMPa1/2 16.1 - 16.916.5
Molar Cohesive Energy EcohJ mol-1 43400 - 4470044100
Glass Transition Temperature TgK 221 - 233226
Molar Heat Capacity Cp J (mol K)-1 292 - 312.5300
Entanglement Molecular Weight Meg mol-1 22400 
Index of Refraction nnone 1.47 - 1.481.47

 1Extrapolated values;  Last updated: May 7, 2018