CROW logo
Poly(cyclohexylethylene)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyalkene (Polyolefin)
COMMON NAMESPoly(cyclohexylethylene), Poly(vinylcyclohexane)
STRUCTURE BASED NAME Poly(cyclohexylethene)
ACRONYMS PVCH
CAS #
CurlySMILES C{-}C{n+}(C1CCCCC1)
 

IDENTIFIERS OF MONOMER(S)

CAS # 695-12-5
COMMON NAMESCyclohexylethylene
SMILES C=CC1CCCCC1
Std. InChI 1S/C8H14/c1-2-8-6-4-3-5-7-8/h2,8H,1,3-7H2
Std. InChIKey LDLDYFCCDKENPD-UHFFFAOYSA-N
STRUCTURE
Cyclohexylethylene
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1116.0 - 119.8117.9
Density ρg mL-1 0.92 - 0.950.94
Solubility Parameter δMPa1/2 16.9
Molar Cohesive Energy EcohJ mol-1 33100
Glass Transition Temperature TgK 393 - 406400
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1 39000 - 4870043000
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 110.20
Van-der-Waals Volume VvWmL mol-1 74.97
Molar Volume VmmL mol-1112.4 - 117.2115.5
Density ρg mL-1 0.94 - 0.980.95
Solubility Parameter δMPa1/2 17.1 - 17.417.2
Molar Cohesive Energy EcohJ mol-1 32700 - 3540034200
Glass Transition Temperature TgK 360 - 399380
Molar Heat Capacity CpJ (mol K)-1145 - 183161
Entanglement Molecular Weight Meg mol-17600 - 108350 44250
Index of Refraction nnone1.49 - 1.511.50

  Last updated: October 6, 2019