Poly(cyanomethyl acrylate)
CROW logo
Poly(cyanomethyl acrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyacrylates
COMMON NAMESPoly(cyanomethyl acrylate)
STRUCTURE BASED NAME Poly(cyanomethyl propenoate)
ACRONYMS PCMA
CAS #
CurlySMILES C{-}C{n+}(C(=O)OCC#N)
 

IDENTIFIERS OF MONOMER(S)

CAS #
COMMON NAMESCyanomethyl acrylate
SMILES C=CC(=O)OCC#N
Std. InChI 1S/C5H5NO2/c1-2-5(7)8-4-3-6/h2H,1,4H2
Std. InChIKey WJMQFZCWOFLFCI-UHFFFAOYSA-N
STRUCTURE
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-182.1
Density ρg mL-1 1.35
Solubility Parameter δMPa1/2 23.8 - 29.726.3
Molar Cohesive Energy EcohJ mol-1 47100 - 7240056600
Glass Transition Temperature TgK 296
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 111.10
Van-der-Waals Volume VvWmL mol-1 57.86
Molar Volume VmmL mol-180.0 - 87.483.2
Density ρg mL-1 1.27 - 1.391.34
Solubility Parameter δMPa1/2 24.1 - 26.725.1
Molar Cohesive Energy EcohJ mol-1 50100 - 5710052200
Glass Transition Temperature TgK 295
Molar Heat Capacity CpJ (mol K)-1137 - 141
181 - 197
141 (s)
190 (l,r)
Entanglement Molecular Weight Meg mol-121000 - 2800024000
Index of Refraction nnone1.49 - 1.511.50
back to top