Poly(butyl vinyl thioether)
CROW logo
Poly(butyl vinyl thioether)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyvinylsulfide
COMMON NAMESPoly(butyl vinyl thioether), Poly(vinyl butyl sulfide)
STRUCTURE BASED NAME Poly(butylthioethylene)
ACRONYMS
CAS #
CurlySMILES C{-}C{n+}(SCCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 4789-70-2
COMMON NAMESButyl vinyl thioether
SMILES CCCCSC=C
Std. InChI 1S/C6H12S/c1-3-5-6-7-4-2/h4H,2-3,5-6H2,1H3
Std. InChIKey LBMGSGLAWRZARD-UHFFFAOYSA-N
STRUCTURE
Butyl vinyl thioether
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1118.6
Density ρg mL-1 0.98
Solubility Parameter δMPa1/2
Molar Cohesive Energy EcohJ mol-1
Glass Transition Temperature TgK 253
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 116.23
Van-der-Waals Volume VvWmL mol-1 71.60
Molar Volume VmmL mol-1111.4 - 116.7116.4
Density ρg mL-1 1.04 - 1.001.00
Solubility Parameter δMPa1/2 17.2 - 17.817.5
Molar Cohesive Energy EcohJ mol-1 34400 - 3650035600
Glass Transition Temperature TgK 254 - 265254
Molar Heat Capacity CpJ (mol K)-1222 - 229225
Entanglement Molecular Weight Meg mol-113000 - 1500015000
Index of Refraction nnone1.53 - 1.541.53