Poly(butyl vinyl ether)
CROW logo
Poly(butyl vinyl ether)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyvinylether
COMMON NAMESPoly(butyl vinyl ether), Poly(vinyl butyl ether)
STRUCTURE BASED NAME Poly(butoxyethylene)
ACRONYMS
CAS #
CurlySMILES C{-}C{n+}(OCCCC)
 

IDENTIFIERS OF MONOMER(S)

CAS # 111-34-2
COMMON NAMESButyl vinyl ether
SMILES CCCCOC=C
Std. InChI 1S/C6H12O/c1-3-5-6-7-4-2/h4H,2-3,5-6H2,1H3
Std. InChIKey IOSXLUZXMXORMX-UHFFFAOYSA-N
STRUCTURE
Poly(butyl vinyl ether)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1108.0 - 111.1109.0
Density ρg mL-1 0.91 - 0.930.92
Solubility Parameter δMPa1/2 16.0 - 23.018.2
Molar Cohesive Energy EcohJ mol-1 27900 - 57700 36100
Glass Transition Temperature TgK 218 - 253220
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone1.46
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 100.16
Van-der-Waals Volume VvWmL mol-1 63.65
Molar Volume VmmL mol-1107.2 - 108.9108.0
Density ρg mL-1 0.92 - 0.930.93
Solubility Parameter δMPa1/2 16.8 - 17.917.2
Molar Cohesive Energy EcohJ mol-1 30700 - 3210031900
Glass Transition Temperature TgK 207 - 225210
Molar Heat Capacity CpJ (mol K)-1205 - 215211
Entanglement Molecular Weight Meg mol-110000 - 1400012500
Index of Refraction nnone1.46 - 1.471.46