POLYMER CLASS | Polycyanoacrylates |
COMMON NAMES | Poly(butyl cyanoacrylate) |
STRUCTURE BASED NAME | Poly(butyl 2-cyanopropenoate), Poly(butyl α‐cyanoacrylate) |
ACRONYMS | |
CAS # | 25154-80-7 |
CurlySMILES | C{-}C{n+}(C#N)(C(=O)OCCCC) |
CAS # | 6606-65-1 |
COMMON NAMES | Butyl 2-cyanoacrylate |
SMILES | CCCCOC(=O)C(=C)C#N |
Std. InChI | 1S/C8H11NO2/c1-3-4-5-11-8(10)7(2)6-9/h2-5H2,1H3 |
Std. InChIKey | JJJFUHOGVZWXNQ-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | ||
Density ρ | g mL-1 | ||
Solubility Parameter δ | MPa1/2 | 19 - 27 | 22.0 |
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 358 - 396 | 374 |
Molar Heat Capacity Cp | J (mol K)-1 | ||
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 153.18 | |
Van-der-Waals Volume VvW | mL mol-1 | 88.70 | |
Molar Volume Vm | mL mol-1 | 128.4 - 134.1 | 130.9 |
Density ρ | g mL-1 | 1.14 - 1.19 | 1.17 |
Solubility Parameter δ | MPa1/2 | 21.2 - 22.8 | 21.8 |
Molar Cohesive Energy Ecoh | J mol-1 | 60100 - 66600 | 62000 |
Glass Transition Temperature Tg | K | 328 - 367 | 344 |
Molar Heat Capacity Cp | J (mol K)-1 | 210 - 222 | 216 |
Entanglement Molecular Weight Me | g mol-1 | 34000 - 50000 | 42000 |
Index of Refraction n | none | 1.50 - 1.51 | 1.50 |
Last updated: April 20, 2017