Poly(benzyl acrylate)
CROW logo
Poly(benzyl acrylate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyacrylates
COMMON NAMESPoly(benzyl acrylate)
STRUCTURE BASED NAME Poly[(phenyl methyl) propenoate]
ACRONYMS
CAS #
CurlySMILES C{-}C{n+}(C(=O)OCc1ccccc1)
 

IDENTIFIERS OF MONOMER(S)

CAS # 2495-35-4
COMMON NAMESBenzyl acrylate
SMILES C=CC(=O)OCc1ccccc1
Std. InChI 1S/C10H10O2/c1-2-10(11)12-8-9-6-4-3-5-7-9/h2-7H,1,8H2
Std. InChIKey GCTPMLUUWLLESL-UHFFFAOYSA-N
STRUCTURE
Benzylacrylate
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1140.9
Density ρg mL-1 1.15
Solubility Parameter δMPa1/2 19.4 - 19.719.5
Molar Cohesive Energy EcohJ mol-1 51100 - 5270051700
Glass Transition Temperature TgK 279 - 284282
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone1.57
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 162.19
Van-der-Waals Volume VvWmL mol-1 91.65
Molar Volume VmmL mol-1133.2 - 138.9135.7
Density ρg mL-1 1.17 - 1.221.19
Solubility Parameter δMPa1/2 20.0 - 20.620.3
Molar Cohesive Energy EcohJ mol-1 53600 - 5730055900
Glass Transition Temperature TgK 350 - 353352
Molar Heat Capacity CpJ (mol K)-1198 - 208
258 - 273
201 (s)
267 (l,r)
Entanglement Molecular Weight Meg mol-131000 - 4000036000
Index of Refraction nnone1.57 - 1.581.57
back to top