Poly(4,4'-thiodiphenylene carbonate)
CROW logo
Poly(4,4'-thiodiphenylene carbonate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polycarbonates
COMMON NAMESPoly(4,4'-thiodiphenylene carbonate)
STRUCTURE BASED NAME Poly(oxycarbonyloxy-1,4-phenylenethio-1,4-phenylene), Poly(oxycarbonyloxy-1,4-phenylenesulfanediyl-1,4-phenylene)
ACRONYMS
CAS #
CurlySMILES O{-}C(=O)Oc1ccc(cc1)Sc1ccc{n+}(cc2)
 

IDENTIFIERS OF MONOMER(S)

CAS # 2664-63-3.75-44-5
COMMON NAMES4,4′-Thiodiphenol, Phosgene
SMILES Oc1ccc(cc1)Sc1ccc(cc1)O.ClC(=O)Cl
Std. InChI 1S/C12H10O2S/c13-9-1-5-11(6-2-9)15-12-7-3-10(14)4-8-12/h1-8,13-14H.1S/CCl2O/c2-1(3)4
Std. InChIKey VWGKEVWFBOUAND-UHFFFAOYSA-N.YGYAWVDWMABLBF-UHFFFAOYSA-N
STRUCTURE
Poly(4,4'-thiodiphenylene carbonate)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1180.2 - 180.3 180.2
Density ρg mL-1 1.36
Solubility Parameter δMPa1/2
Molar Cohesive Energy EcohJ mol-1
Glass Transition Temperature TgK 383 - 388386
Molar Heat Capacity CpJ (mol K)-1
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 244.27
Van-der-Waals Volume VvWmL mol-1 120.01
Molar Volume VmmL mol-1175.0 - 181.6178.3
Density ρg mL-1 1.35 - 1.401.37
Solubility Parameter δMPa1/2 22.0 - 22.422.3
Molar Cohesive Energy EcohJ mol-1 86500 - 9050088400
Glass Transition Temperature TgK 381
Molar Heat Capacity CpJ (mol K)-1255 - 262259
Entanglement Molecular Weight Meg mol-12500 - 27502600
Index of Refraction nnone1.63 - 1.691.67
back to top