Poly(4-fluorostyrene)
CROW logo
Poly(4-fluorostyrene)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyhalostyrene
COMMON NAMESPoly(4-fluorostyrene)
STRUCTURE BASED NAME Poly[1-(4-fluorophenyl)ethane-1,2-diyl], Poly(4-fluorophenylethylene)
ACRONYMS
CAS #
CurlySMILES C{-}C{n+}(c1ccc(F)cc1)
 

IDENTIFIERS OF MONOMER(S)

CAS # 24936-47-8
COMMON NAMES
SMILES C=Cc1ccc(cc1)F
Std. InChI 1S/C8H7F/c1-2-7-3-5-8(9)6-4-7/h2-6H,1H2
Std. InChIKey JWVTWJNGILGLAT-UHFFFAOYSA-N
STRUCTURE
Poly(4-fluorostyrene)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1102.0
Density ρg mL-1 1.20
Solubility Parameter δMPa1/2 18.3 - 19.118.8
Molar Cohesive Energy EcohJ mol-1 34200 - 3720036000
Glass Transition Temperature TgK 368 - 384376
Molar Heat Capacity CpJ (mol K)-1117
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 122.14
Van-der-Waals Volume VvWmL mol-1 67.92
Molar Volume VmmL mol-1102.3 - 108.2105.1
Density ρg mL-1 1.13 - 1.191.16
Solubility Parameter δMPa1/2 17.9 - 18.718.3
Molar Cohesive Energy EcohJ mol-1 34100 - 3590035100
Glass Transition Temperature TgK 386 - 402394
Molar Heat Capacity CpJ (mol K)-1123 - 141130
Entanglement Molecular Weight Meg mol-114000 - 2000018000
Index of Refraction nnone1.55 - 1.571.56