Poly(4-bromostyrene)
CROW logo
Poly(4-bromostyrene)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyhalostyrene
COMMON NAMESPoly(4-bromostyrene)
STRUCTURE BASED NAME Poly[1-(4-bromophenyl)ethane-1,2-diyl], Poly(4-bromophenylethylene)
ACRONYMS
CAS # 24936-50-3
CurlySMILES C{-}C{n+}(c1ccc(cc1)Br)
 

IDENTIFIERS OF MONOMER(S)

CAS # 2039-82-9
COMMON NAMES
SMILES C=Cc1ccc(cc1)Br
Std. InChI 1S/C8H7Br/c1-2-7-3-5-8(9)6-4-7/h2-6H,1H2
Std. InChIKey WGGLDBIZIQMEGH-UHFFFAOYSA-N
STRUCTURE
Poly(4-bromostyrene)
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1119.0
Density ρg mL-1 0.87
Solubility Parameter δMPa1/2 18.6 - 20.219.7
Molar Cohesive Energy EcohJ mol-1 41100 - 4840046000
Glass Transition Temperature TgK 391 - 430411
Molar Heat Capacity CpJ (mol K)-1140
Entanglement Molecular Weight Meg mol-130000
Index of Refraction nnone
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 103.14
Van-der-Waals Volume VvWmL mol-1 78.81
Molar Volume VmmL mol-1118.4 - 118.9118.7
Density ρg mL-1 0.870.87
Solubility Parameter δMPa1/2 19.6 - 20.620.2
Molar Cohesive Energy EcohJ mol-1 45800 - 5010048600
Glass Transition Temperature TgK 358 - 423391
Molar Heat Capacity CpJ (mol K)-1140 - 155148
Entanglement Molecular Weight Meg mol-117000 - 3500027000
Index of Refraction nnone1.61 - 1.621.62
back to top